ADVANCE

Product images

TEROSON

TEROSON MS 939NA

Product codeMS 939NA

SubcategoryMS Polymer Adhesives & Sealants

MS Polymer Adhesives & SealantsAdhesives

High-strength, high-elongation one-part MS Polymer for primerless elastic bonding and sealing, with functional strength in 24 hours and full cure in 7 days.

Find AdhesiveRequest RFQ

Images and data on this page are for reference. Packaging and specifications may change by the manufacturer. Please check the latest TDS or contact our team before ordering.

Product overview

TEROSON MS 939NA is used for elastic bonding and sealing on a wide range of substrates, including steel, stainless steel, aluminum, glass, wood, polycarbonate, PVC and ABS, with no primer needed. It is a one-part modified silane polymer in black, white or grey. It combines strength with stretch: 2.7 N/mm² tensile strength and 500% elongation after 3 days at 22 °C, with Shore A hardness of 52 to 62. Sag resistance gives high initial tack. It is odorless, non-corrosive and free of solvents, isocyanates, silicones and PVC, and it works with suitable paint systems. UV resistance allows interior and exterior use. It cures with atmospheric moisture and skins over in 3 to 12 minutes at 25 °C and 50% humidity, so mate parts within a few minutes of dispensing. Functional strength comes in 24 hours and full cure in 7 days. Store at 8 to 21 °C. It does not adhere to polyethylene, polypropylene or PTFE, should not be used on PMMA or polycarbonate under tension, and is not for pure oxygen or strong oxidizers.

Features & applications

Key features

  • High strength and high elongation: 2.7 N/mm² tensile and 500% elongation after 3 days at 22 °C
  • Functional strength in 24 hours, full cure in 7 days
  • Adheres without primer to a wide variety of substrates
  • Sag resistant, which gives high initial tack
  • Odorless, non-corrosive, free of solvents, isocyanates, silicones and PVC

Applications & Industries

Application

  • Elastic bonding on steel, stainless steel, galvanized steel and aluminum
  • Bonding glass, wood, polycarbonate, PVC and ABS
  • Interior and exterior sealing, including painted joints

Industries

  • Industrial Manufacturing

Product specifications

Technical data

PropertyValueUnit
ColorBlack; white; grey—
Density1.3 to 1.6g/ml
Tensile strength2.7N/mm²
Elongation500%
Material: Modified silane polymerModified silane polymer—
Skin-over time at 25 °C, 50% humidity3 to 12min
Shore A hardness, cured 3 days at 22 °C52 to 62—
Lap shear on grit-blasted steel, cured 21 days at 22 °C1.9N/mm²

Packaging / SKU

SizePackaging
570 ml—
55 gal—
290 ml—

Ask about MS 939NA

Find alternatives, compare with another product, or ask a spec from the TDS.

Technical Documents

  • Technical Data Sheet

    Technical Data Sheet · EN · Rev v01 · teroson-ms-939na

  • Safety Data Sheet

    Safety Data Sheet · EN · Rev v01 · teroson-ms-939na