Non-silicone polyester thermal insulator on polyimide film, 1.3 W/(m·K), 0.6 °C·in²/W at 50 psi and 6000 VAC, for silicone-sensitive power assemblies.

Find AdhesiveRequest RFQ

Images and data on this page are for reference. Packaging and specifications may change by the manufacturer. Please check the latest TDS or contact our team before ordering.

Product overview

BERGQUIST SIL PAD TSP PPK1300, formerly BERGQUIST POLY-PAD K-10, is a thermal insulator made of polyimide film coated with a ceramic-filled polyester resin. It is meant for critical silicone-sensitive work: assemblies that receive non-silicone conformal coatings, or where silicone contamination is a concern, as in telecom and some aerospace equipment. Typical uses are power supplies, motor controls and power semiconductors. Thermal conductivity is 1.3 W/(m·K) and thermal impedance is 0.6 °C·in²/W at 50 psi. Dielectric breakdown voltage is 6000 VAC and volume resistivity is 1×10^12 Ω·m. The yellow pad is 0.152 mm thick, hardness is 90 Shore A and the operating range is -20 to 150 °C. Supplied as sheets, rolls and die-cut parts, with or without pressure-sensitive adhesive.

Features & applications

Key features

  • Thermal conductivity 1.3 W/(m·K)
  • Thermal impedance 0.6 °C·in²/W at 50 psi
  • Dielectric breakdown voltage 6000 VAC
  • Non-silicone polyester resin on polyimide film, 0.152 mm
  • TO-220 thermal performance 2.75 °C/W at 50 psi

Applications & Industries

Application

  • Power supplies
  • Motor controls
  • Power semiconductors
  • Assemblies with non-silicone conformal coating or a silicone contamination concern

Industries

  • Power electronics
  • Industrial electronics

Product specifications

Technical data

PropertyValueUnit
TechnologyPolyester-based—
ColorYellow—
Operating temperature-20 to 150°C
Thermal conductivity1.3W/(m·K)
Volume resistivity1×10^12Ω·m
Standard thickness0.152mm
Reinforcement carrierPolyimide film—
Dielectric breakdown voltage6000VAC
Thermal impedance at 10 psi1.04°C·in²/W
Former nameBERGQUIST POLY-PAD K-10—

Ask about SIL PAD TSP PPK1300

Find alternatives, compare with another product, or ask a spec from the TDS.

Technical Documents

  • Technical Data Sheet

    Technical Data Sheet · EN · Rev v01 · bergquist-sil-pad-tsp-ppk1300

Need a technical recommendation or quotation?

Tell us about the application, substrate, packaging, and production requirements. Our team will follow up on qualified RFQs.

Request an RFQ