ADVANCE
Back to Detail & Suggestion

PCB materials

Electrically Conductive Film Adhesives for PCB and Display Assembly

Electrically conductive film adhesives replace solder or liquid conductive paste where parts must be joined under heat and pressure with a controlled, uniform bond line. They are the standard choice for flexible circuit to glass, flex to rigid board and fine-pitch driver connections.

Illustration of electrically conductive film adhesives on a PCB assembly

What it is and its role in the assembly

An electrically conductive film adhesive is a solid, pre-formed adhesive layer, usually an epoxy or acrylic matrix, filled with conductive particles and supplied on a release liner. It is cut or slit to the joint size, placed between two conductor surfaces and bonded under heat and pressure. During bonding the matrix softens, flows around the particles and then cures, so the finished joint is both a mechanical bond and an electrical path.

In an assembly it replaces a solder joint, a connector or a liquid conductive adhesive wherever the parts cannot tolerate reflow temperature, where pitch is too fine for paste, or where the joint must stay thin and flat. Because the film is solid, there is no dispensing, no bleed and no need to control a wet thickness.

Where it is used on a PCB

The largest use is in display and touch modules, where flexible printed circuits and driver ICs are bonded to glass or to the main board. The same approach is used wherever a flexible circuit meets a rigid board, a sensor tail joins an electronics module, or a shielding layer must be grounded along a seam.

  • Flex on glass (FOG) and chip on glass (COG) joints in LCD and OLED modules
  • Flex on board (FOB) connections in smartphones, tablets, cameras and wearables
  • Touch sensor tails and fingerprint or biometric sensor modules
  • Automotive displays and instrument clusters where vibration rules out connectors
  • Grounding of EMI shields and bonding of printed electronics on flexible substrates
  • RFID and smart card inlays where a chip is bonded to a printed antenna

Problems it solves and why it matters

Fine-pitch connections at 100 micrometers and below cannot be soldered or dispensed reliably, and glass, polyester and many polyimide builds cannot survive reflow. A film adhesive bonds at a lower temperature, with its thickness fixed by the film rather than by the operator, and with a mechanical bond that spreads load across the whole joint area rather than concentrating it on individual solder fillets.

The result is a joint that resists vibration and flex fatigue, keeps contact resistance stable through thermal cycling and humidity, and can be processed in a repeatable, inspectable way on automated bonders. For process yield, the absence of solder balls, bridging and paste slump is often the deciding factor.

  • Fine-pitch electrical connection without solder bridging
  • Lower bonding temperature than reflow, suitable for glass and heat-sensitive films
  • Uniform bond line thickness set by the film, not by dispensing
  • Stable contact resistance under thermal cycling, humidity and flexing
  • Clean, lead-free joint with no flux residue to clean

Chemistries and product types

The main distinction is how the film conducts. Anisotropic conductive film (ACF) contains a low loading of conductive particles, so it conducts only in the Z direction between the two electrodes that trap particles under pressure, while neighboring electrodes stay insulated. Isotropic conductive film (ICF) is filled heavily enough to conduct in all directions and is used for ground straps, shield attachment and larger pad-to-pad bonds where no fine pitch is involved.

Within each family the matrix chemistry sets the process window. Thermosetting epoxy films give the highest bond strength and heat resistance but need a defined temperature and time to cure. Thermoplastic and pressure-sensitive variants bond faster and can be reworked, at the cost of lower temperature resistance. Particle systems range from solid metal powders to polymer spheres plated with nickel and gold, and the carrier may be a single layer film or a dual layer with a non-conductive flow layer.

  • Anisotropic conductive film (ACF): Z-axis conduction for fine pitch, FOG, COG and FOB
  • Isotropic conductive film (ICF): all-direction conduction for grounding and shielding
  • Thermoset epoxy matrix for strength and heat resistance; thermoplastic or acrylic for fast, reworkable bonds
  • Particle types: metal-coated polymer spheres, nickel, silver or solder-based particles
  • Carrier formats: single-layer film, dual-layer film, tape on reel, pre-cut pieces

Key properties to specify

The specification starts with the joint geometry: minimum pitch, pad width, bump height and the bonded area. From there the key figures are the connection resistance per bump after bonding, the insulation resistance between adjacent pads, the peel or shear strength on the actual substrate pair, and the bonding profile the material needs. Film thickness is typically chosen in the range of 15 to 50 micrometers so that the film fills the gap between bumps without squeezing out.

Reliability figures should be quoted after conditioning, not only as initial values. Ask for resistance change after thermal cycling, high temperature and humidity storage, and bend testing if the joint is on a flexible circuit. Shelf life and storage temperature matter more than for most adhesives, because reactive films are often stored cold and have a limited time at room temperature.

  • Minimum pitch and pad geometry the film is rated for
  • Connection resistance per joint, typically in the tens of milliohms for ACF bumps
  • Insulation resistance between adjacent conductors, often specified above 10 to the power of 8 ohms
  • Film thickness and particle size relative to bump height
  • Bonding temperature, pressure and time; a pre-bond or tack stage if needed
  • Peel strength on the real substrate pair, for example polyimide to glass or to FR-4
  • Tg and continuous operating temperature after cure
  • Shelf life, storage temperature and allowed time out of refrigeration

Application and processing

Processing follows a fixed sequence: the film is laminated to one side of the joint at low temperature and pressure (pre-bond), the liner is removed, the second part is aligned under a vision system, and the main bond is made with a heated tool head at the final temperature, pressure and time. For ACF, the pressure stage is what deforms the particles between the electrodes and makes the electrical contact, so pressure uniformity across the tool head is as important as temperature.

Thermocompression bonders with constant-heat or pulse-heat heads are the usual equipment. A compliant buffer sheet such as silicone rubber or PTFE between the head and the part evens out pressure over uneven surfaces. Production is in-line and cycle times are short, usually seconds per joint, which makes the bonding profile the main lever for both throughput and quality.

  • Pre-bond: low temperature and pressure for a few seconds to tack the film in place
  • Liner removal and vision alignment of the mating part
  • Main bond: heated head at the specified temperature, pressure and time
  • Buffer sheet between head and part to equalize pressure
  • Inspection: particle deformation count through glass, resistance test, peel test on coupons

Design and process considerations

Pad finish and cleanliness decide adhesion and contact resistance. Gold, tin or ITO surfaces bond well when free of organics; oxidized copper and residues from solder mask or plasma processes do not. Pad and bump design should keep enough area per joint for several trapped particles, and the substrates should be flat enough that the tool head can apply even pressure. On flexible circuits, a stiffener behind the bond area keeps the joint from flexing at the adhesive edge.

Thermal expansion mismatch between glass, polyimide and FR-4 shifts pad positions during heating, so the bonding temperature and the alignment offset need to be set together. Rework is possible for most films by heating and peeling, followed by solvent cleaning of the residue, but the pads only tolerate a limited number of cycles and the process should be qualified rather than assumed.

  • Clean pads with plasma or solvent before lamination; no fingerprints or mask residue
  • Match film thickness to bump height and pad step
  • Keep the bond area flat; use stiffeners on flex and avoid vias under the joint
  • Compensate for thermal expansion when setting alignment offsets
  • Qualify rework: number of cycles, cleaning method, pad condition after removal

Common defects and how to avoid them

Most defects trace back to the bonding profile or to the surfaces. Open or high-resistance joints come from too little pressure, too few particles under the pad, misalignment or contaminated pads. Shorts between adjacent pads come from excessive particle loading, too much pressure forcing particles sideways, or a film that is too thick for the pitch. Bubbles and voids in the adhesive come from trapped air during pre-bond, moisture in the substrate or a temperature that rises too fast before the resin has flowed.

  • Open joints: raise pressure within the specified window, verify flatness and particle count, check pad cleanliness
  • Shorts: confirm pitch rating, reduce pressure or film thickness, check alignment
  • Voids and bubbles: bake moisture-sensitive substrates, slow the temperature ramp, improve head contact
  • Delamination after reliability test: incomplete cure, contaminated surfaces or CTE mismatch at the edge
  • Resin squeeze-out onto neighboring areas: too much film width or pressure
  • Drift between lots: film stored too long at room temperature or past shelf life

How to select the right product and what to tell ADVANCE

Film selection is driven by the joint, the substrates and the bonder you already have. Send us the geometry and the two surfaces first; the chemistry follows from there. Where the application is new, we recommend a sample trial on your production bonder with resistance and peel measurements before and after thermal cycling, and we provide the TDS and SDS for every candidate so that your process and safety teams can review them in parallel.

  • Joint type: FOG, COG, FOB, flex to flex, grounding or shield attachment
  • Substrates and pad finishes on both sides, for example ITO glass, gold on polyimide, ENIG on FR-4
  • Minimum pitch, pad size, bump height and number of connections
  • Maximum temperature the parts tolerate and the operating temperature range of the product
  • Bonder type, head size, available pressure and takt time
  • Reliability tests required: thermal cycling, high temperature and humidity, bend or vibration
  • Rework expectations and any restricted substances
  • Format preferred: reel width and length, or pre-cut pieces

Products to consider

  • LOCTITE ABLESTIK CF 3350

    LOCTITE

    LOCTITE ABLESTIK CF 3350

    Product code: ABLESTIK CF 3350

    Silver-filled epoxy film that bonds circuit boards to metal backplanes and heat sinks, conducting both electricity and heat through the bond.

  • LOCTITE ABLESTIK ECF 550X

    LOCTITE

    LOCTITE ABLESTIK ECF 550X

    Product code: ABLESTIK ECF 550X

    Silver-filled epoxy film on glass fabric that conducts in all three axes. Used for substrate attach, where it also acts as an electrical ground plane.

  • LOCTITE ABLESTIK 5025E

    LOCTITE

    LOCTITE ABLESTIK 5025E

    Product code: ABLESTIK 5025E

    Silver-filled conductive epoxy film for attaching hot devices to heat sinks and for microwave circuits. Conducts in all three axes, gives RF/EMI shielding.

  • LOCTITE ABLESTIK CDF 500

    LOCTITE

    LOCTITE ABLESTIK CDF 500

    Product code: ABLESTIK CDF 500

    Conductive die attach film for ICs and components on metal leadframes, with a consistent bondline, a controlled fillet and no resin bleed-out.

View all 117 Electronic Assembly Adhesives →

Frequently asked questions

What is the difference between ACF and ICF?
ACF conducts only through the film thickness, between the two pads that press on the same particles, so adjacent pads stay insulated and fine pitch is possible. ICF conducts in every direction and is used for ground straps, shield attachment and large single pads. Using ICF on a fine-pitch connector would short the pads.
Can a film adhesive joint be reworked?
Usually yes. The joint is heated to soften the matrix, the flex is peeled off and the residue is removed with a suitable solvent or by gentle mechanical cleaning, then a new film is bonded. The number of rework cycles is limited by the pad finish, especially on ITO glass, so qualify the procedure on scrap parts and set a maximum count.
How should conductive films be stored and handled?
Reactive epoxy films are normally stored refrigerated and have a defined shelf life plus a limited allowance at room temperature. Let the reel reach room temperature in its sealed bag before opening, to avoid condensation on the film. Record the date the reel is opened and the cumulative hours out of cold storage, and keep the liner on until just before lamination.
How do I check an ACF bond without destroying it?
On glass, deformed particles can be counted through the substrate under a microscope; a stable count per pad is a good in-process indicator. Electrical tests measure connection resistance and insulation resistance on test pads or the daisy chain of the product. Peel and shear tests remain destructive and are run on coupons at set intervals and after any profile change.

Need a conductive film for a flex or display joint?

Send us the pad geometry, both substrates and your bonder details. We will propose candidate films with TDS and SDS, and arrange samples for a trial on your line or an RFQ for production quantities.

Not sure which product fits? Ask our assistant