ADVANCE
Back to Detail & Suggestion

PCB materials

Phase Change Materials and Thermal Greases for Component-to-Heatsink Interfaces

Thermal greases and phase change materials are the thinnest class of thermal interface material. They are used where a component or a metal-backed board is clamped to a heatsink and the only job of the interface is to replace trapped air in the surface roughness with something that conducts heat.

Illustration of phase change materials and thermal greases on a PCB assembly

What it is and its role in the assembly

A thermal grease is a paste of thermally conductive filler such as zinc oxide, alumina, boron nitride or metal particles in a silicone or synthetic oil carrier. It never cures and stays a paste for the life of the product. A phase change material (PCM) is a similar filled compound formulated as a wax-like solid at room temperature; above its phase change temperature, typically around 45 to 60 degrees Celsius, it softens and flows like a grease, wets both surfaces under clamping pressure and then stays in place.

Both sit between two surfaces that are already pressed together by screws, clips or springs. They carry no mechanical load and provide no adhesion; their role is purely to fill a thin, uneven gap, usually below 100 micrometers, with a low thermal resistance layer. The clamp holds the parts; the interface only makes the contact thermally effective.

Where it is used on a PCB

The typical location is any clamped interface with a small, controlled gap: a processor or power module lid to a heatsink, a TO-247 or TO-220 package to a heatsink or chassis, or the back of an insulated metal substrate to a housing. Greases dominate where the parts are serviced and reassembled; phase change pads are preferred where a dry, pre-applied material simplifies assembly and removes the mess of paste.

  • CPU, GPU and FPGA lids to heatsinks in servers, networking and industrial computers
  • Discrete power packages (TO-220, TO-247, D2PAK on tabs) clamped to heatsinks in power supplies and motor drives
  • IGBT and MOSFET power modules on cold plates in inverters, chargers and traction systems
  • IMS LED boards and automotive ECU boards bolted to housings
  • Telecom radio units, base station amplifiers and optical modules
  • Battery modules and charging electronics where cells or boards meet a cooling plate

Problems it solves and why it matters

Two metal surfaces that look flat touch only at a few high points; most of the apparent contact area is air, and air is an excellent insulator. A bare clamped joint can have a thermal resistance several times higher than the same joint with a thin layer of grease, which translates directly into tens of degrees at the junction. Filling that gap is the cheapest thermal improvement available in most designs.

Compared with thicker gap pads, greases and PCMs reach a much lower thermal resistance because the bond line is thin and they need little clamping force to conform. Phase change materials add two production benefits: they are applied dry as a pad or screen-printed film, so there is no wet paste on the line, and once they have gone through their first thermal cycle they resist pump-out better than many greases.

  • Replaces trapped air at the interface with a conducting layer
  • Lowest thermal resistance of the common interface materials at thin bond lines
  • Conforms at low clamping pressure, protecting packages from mechanical stress
  • PCM pads give clean, dry, repeatable application on the line
  • Serviceable: the joint can be opened, cleaned and re-applied

Chemistries and product types

Greases are divided first by carrier. Silicone greases are the most widely used because the oil is stable over a wide temperature range and wets metals well; the drawback is low molecular weight siloxane that can migrate and contaminate optical surfaces or interfere with later bonding and coating steps. Non-silicone greases use synthetic hydrocarbon or ester oils for silicone-free assemblies, usually with a narrower temperature range. The filler sets the conductivity: ceramic fillers for electrical insulation, metal fillers such as aluminum or silver for higher conductivity but electrical conductivity as well.

Phase change materials are supplied as pads with a release liner, as pre-cut shapes, as coated films on a carrier for high-power modules, or as screen-printable or dispensable compounds that are dried onto the heatsink. The phase change temperature is chosen slightly below the normal operating temperature of the component so the material softens in service but stays solid during storage and handling. Some grades include a carrier mesh or a thin metal foil for easier handling of large pads.

  • Silicone grease: widest temperature range, best wetting, siloxane migration risk
  • Non-silicone grease: for silicone-free lines, optics and pre-coating steps
  • Ceramic-filled (insulating) versus metal-filled (higher conductivity, electrically conductive)
  • Phase change pads and die-cut shapes with liner
  • Phase change coated foils for large power modules
  • Printable or dispensable phase change compounds applied to the heatsink
  • Phase change temperature typically 45 to 60 degrees Celsius

Key properties to specify

The property that matters is thermal impedance, the resistance of the whole layer at a stated thickness and pressure, not bulk thermal conductivity alone. A grease with moderate conductivity at a 25 micrometer bond line will outperform a higher conductivity product that cannot be spread thinner than 100 micrometers. Ask for thermal impedance at the clamping pressure your design actually provides, and for the bond line thickness it was measured at.

For greases, viscosity and the oil separation or bleed figure predict how the material will behave in dispensing and over time. For phase change materials, the phase change temperature, the minimum pressure needed to achieve full wet-out and the behavior after repeated cycles are the decisive points. Both types need an operating temperature range, an electrical classification and, for automotive and sealed enclosures, outgassing and silicone content statements.

  • Thermal impedance at a stated thickness and pressure, often quoted in square centimeter kelvin per watt
  • Bulk thermal conductivity, typically in the range of 1 to 6 W per meter kelvin for filled greases
  • Achievable bond line thickness at the available clamping pressure
  • Operating temperature range and phase change temperature for PCMs
  • Volume resistivity and dielectric strength if the interface must insulate
  • Viscosity, oil bleed and evaporation loss for greases
  • Silicone content, outgassing and UL 94 rating where the enclosure requires it
  • Shelf life and storage conditions, especially for pre-applied PCM pads

Application and processing

Grease is applied by screen or stencil printing on the heatsink, by automated dispensing of a dot, line or pattern, or by hand with a spatula or roller in low volumes. The goal is the thinnest continuous layer that still fills the gap after clamping, which usually means a defined pattern that spreads to full coverage under pressure rather than a thick uniform coat. Automated lines use volumetric dispensers with pattern recognition so the amount per part is logged.

Phase change pads are peeled from the liner and placed on the heatsink or the component, by hand or by pick and place, then the assembly is clamped. Full wet-out happens on the first warm-up in service or during a deliberate burn-in, so the thermal resistance measured straight after assembly is higher than the final value. Printed phase change compounds are applied to heatsinks by the heatsink supplier and arrive dry and ready. Inspection on the line is mostly visual for coverage plus weight or dispense volume checks; thermal impedance is verified on samples with a test fixture.

  • Grease: stencil or screen printing for repeatable thickness on flat heatsinks
  • Grease: automated dispensing in a pattern sized to spread to full coverage under clamp
  • PCM: pad placement by hand or pick and place, then clamp; wet-out on first heating
  • PCM: printed compound pre-applied to the heatsink and dried
  • Clamp with the specified torque sequence to achieve the designed pressure
  • Inspection: coverage, dispense weight, sample thermal impedance, optional burn-in

Design and process considerations

The clamping design is part of the thermal design. Pressure must be high enough and evenly distributed for the material to spread thin, and the surfaces should be flat and clean; machining marks, anodizing and residual oils all raise the final thermal resistance. Where a lid or heatsink bows under the clamp, the center gap grows and the interface may need to be thicker or replaced by a gap filler.

Pump-out and dry-out are the long-term failure modes. Repeated thermal cycling makes the two surfaces move relative to each other, squeezing grease out of the gap; over years, the oil can also separate or evaporate and leave a dry, cracked filler. Products differ widely in their resistance to these effects, and phase change materials generally hold up better once wetted. Silicone compatibility with adjacent processes, such as conformal coating or adhesive bonding, must be checked before a silicone grease is introduced to the line. Rework is simple in principle, clean and re-apply, but the cleaning solvent and lint-free procedure should be written down.

  • Design clamping pressure and torque sequence together with the interface material
  • Specify surface flatness and roughness on both mating parts; degrease before assembly
  • Check bowing of lids and heatsinks under clamp; use a gap filler if the gap exceeds the material range
  • Qualify pump-out and dry-out with thermal cycling and high temperature storage on the real geometry
  • Keep silicone greases away from optics, coating lines and bonding surfaces
  • Write a rework procedure: solvent, wipe, inspection, re-application amount

Common defects and how to avoid them

Most field returns with an overheated component trace back to the interface rather than the heatsink: too little material leaving dry patches, too much material forming a thick layer that never thinned out, air trapped in a uniform coat, grease pumped out of a cycling joint, or a phase change pad that was never clamped hard enough to wet the surface. On the line, contamination of the grease with dust or lint, and pads placed off-center or with the liner still on, are the recurring causes.

  • Dry spots and voids: use a dispense pattern that spreads to full coverage, confirm with a pull-apart check on samples
  • Thick bond line: reduce the amount, raise clamping pressure, verify flatness
  • Pump-out after cycling: choose a grease rated for pump-out resistance or switch to a phase change material
  • Dry-out and cracking: select a low-bleed formulation and qualify with high temperature storage
  • Incomplete PCM wet-out: check minimum pressure, confirm the pad reaches its phase change temperature, add a burn-in step
  • Contamination: closed cartridges, lint-free wipes, cleaned fixtures, no touching the applied layer
  • Silicone contamination of downstream processes: isolate the application station and verify with a wetting test

How to select the right product and what to tell ADVANCE

The decision between grease and phase change material, and then between grades, follows from the gap, the pressure and the service life you need. A thin, flat, well-clamped joint that is never reopened suits a phase change pad; a serviced joint or one with a large production volume on existing dispensing equipment usually suits a grease. Give us the geometry and the environment, and we will shortlist candidates with TDS and SDS and arrange samples so you can measure thermal impedance on your own fixture before committing to a volume RFQ.

  • Component or module type, contact area and the power to be removed
  • Gap range, surface flatness and finish of both parts, clamping pressure available
  • Operating and storage temperature range, number of thermal cycles expected
  • Electrical requirement: insulating or not, any clearance to live parts
  • Silicone allowed or not, outgassing limits, sealed enclosure
  • Application method on your line: print, dispense, pad placement, and the takt time
  • Serviceability: will the joint be opened for repair
  • Reliability tests required: thermal cycling, high temperature storage, humidity, vibration

Products to consider

  • BERGQUIST HI FLOW THF 500

    BERGQUIST

    BERGQUIST HI FLOW THF 500

    Product code: HI FLOW THF 500

    Electrically isolating phase change pad on PEN film for spring or clip mounted power semiconductors and modules, with 4000 VAC breakdown voltage.

  • BERGQUIST HI FLOW THF 900

    BERGQUIST

    BERGQUIST HI FLOW THF 900

    Product code: HI FLOW THF 900

    Aluminum carrier coated on both sides with phase change compound, a clean replacement for thermal grease where electrical isolation is not needed.

  • BERGQUIST HI FLOW THF 1500P

    BERGQUIST

    BERGQUIST HI FLOW THF 1500P

    Product code: HI FLOW THF 1500P

    Electrically insulating phase change pad on polyimide film for power semiconductors and modules that must be isolated from the heat sink. Phase change at 52 °C.

  • BERGQUIST HI FLOW THF 1600P

    BERGQUIST

    BERGQUIST HI FLOW THF 1600P

    Product code: HI FLOW THF 1600P

    Electrically insulating phase change pad on polyimide film for power devices that need isolation from the heat sink, with 5000 VAC breakdown voltage.

  • BERGQUIST HI FLOW THF 3000UT

    BERGQUIST

    BERGQUIST HI FLOW THF 3000UT

    Product code: HI FLOW THF 3000UT

    Tacky, unreinforced blue phase change pad for processor lids, dies and memory modules, with 3.0 W/(m·K) thermal conductivity.

  • BERGQUIST HI FLOW THF 3500U

    BERGQUIST

    BERGQUIST HI FLOW THF 3500U

    Product code: HI FLOW THF 3500U

    Unreinforced gray phase change pad with 3.5 W/(m·K) thermal conductivity for processor lids, dies and memory module heat spreaders.

  • LOCTITE TCP 4000 PM

    LOCTITE

    LOCTITE TCP 4000 PM

    Product code: TCP 4000 PM

    Reworkable phase change paste, printed, dispensed or applied by hand, then dried to a solid film. It flows at 45 °C to fill the gap between processors and heat sinks.

  • LOCTITE TCP 7000

    LOCTITE

    LOCTITE TCP 7000

    Product code: TCP 7000

    Non-silicone phase change paste, stencil or screen printed and dried to a solid film. Above 45 °C it flows to fill the interface between processors and heat sinks.

  • LOCTITE TG 100

    LOCTITE

    LOCTITE TG 100

    Product code: TG 100

    Gray silicone thermal grease for CPUs, GPUs and power components, with 3.4 W/(m·K) thermal conductivity and an operating range of -40 to 150 °C.

  • BERGQUIST TGR 4000

    BERGQUIST

    BERGQUIST TGR 4000

    Product code: TGR 4000

    Gray silicone thermal grease for the interface between a processor and a copper heat sink, with 4.0 W/(m·K) thermal conductivity. It flows under clamping pressure and does not drip.

  • BERGQUIST HI FLOW THF 700UT

    BERGQUIST

    BERGQUIST HI FLOW THF 700UT

    Product code: HI FLOW THF 700UT

    Unreinforced, naturally tacky phase change pad, 0.077 mm thick, for high performance processors, graphics cards and power modules.

  • BERGQUIST HI FLOW THF 1600G

    BERGQUIST

    BERGQUIST HI FLOW THF 1600G

    Product code: HI FLOW THF 1600G

    Green phase change pad on a fiberglass carrier for the interface between a computer processor and its heat sink, 0.127 mm thick.

View all 78 Thermal Management →

Frequently asked questions

Grease or phase change material: which should I use?
Use a phase change pad when the joint is assembled once, the gap is thin and controlled, and you want a clean, dry process with good pump-out resistance. Use a grease when the joint will be serviced, when the surface is irregular enough to need a paste that flows at room temperature, or when you already dispense on the line. Thermal performance of the two is similar at the same bond line thickness.
How much grease should be applied?
As little as will still give full coverage after clamping. Calculate the volume from the contact area and a target bond line, typically a few tens of micrometers, then verify by clamping a sample, pulling it apart and checking that the print covers the whole pad without heavy squeeze-out at the edges. Lock the dispense weight or stencil thickness once it is confirmed.
Why does the thermal resistance of a phase change pad look high right after assembly?
At room temperature the pad is solid and only touches the high points of both surfaces. It has to be heated past its phase change temperature under clamping pressure before it flows into the roughness and reaches its rated impedance. A burn-in step, or simply the first hours of normal operation, completes the wet-out; measure after that, not before.
Can a silicone grease cause problems elsewhere in the product?
It can. Volatile siloxanes migrate and settle on nearby surfaces, which can cause poor wetting of conformal coatings and adhesives, fish-eyes in paint and contamination of optical windows or connector contacts in sealed enclosures. If any of these are present, use a low-volatility silicone grade or a non-silicone grease, apply it at a separate station and verify downstream wetting on a trial build.

Need to lower the thermal resistance of a clamped joint?

Tell us the contact area, gap, clamping pressure and temperature range. We will shortlist greases or phase change materials, send TDS and SDS, and provide samples for impedance testing on your fixture before you raise an RFQ.

Not sure which product fits? Ask our assistant